密度 | 1.15g/cm3 | 熔體流動(dòng)速率 | 30g/10min | 吸水率 | 0.3% |
缺口沖擊強(qiáng)度 | 12 | 成型收縮率 | 0.55% |
|
產(chǎn)品簡述
密度 | 1.15g/cm3 | 熔體流動(dòng)速率 | 30g/10min | 吸水率 | 0.3% |
缺口沖擊強(qiáng)度 | 12 | 成型收縮率 | 0.55% |
詳細(xì)數(shù)據(jù)
訂購指南
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
物理性能 | 熔體流動(dòng)速率 | 200℃ 21.6kg | ASTM D-1238 | 30 | g/10min | |
模塑收縮率 | ASTM D-955 | 0.4-0.7 | % | |||
比重 | ASTM D-792 | 1.15 | ||||
吸水性 | ASTM D-570 | 0.3 | % | |||
機(jī)械性能 | 缺口沖擊強(qiáng)度 | 厚度6.4mm 缺口 | ASTM D-256 | 12.0 | kg.cm/cm | |
拉伸強(qiáng)度 | ASTM D-638 | 500 | kg/cm2 | |||
彎曲強(qiáng)度 | ASTM D-790 | 700 | kg/cm2 | |||
洛氏硬度 | ASTM D-785 | 103 | R | |||
伸長率 | ASTM D-638 | 30 | % | |||
彎曲模量 | ASTM D-790 | 25000 | kg/cm2 | |||
電氣性能 | 介電常數(shù) | ASTM D-150 | 2.8↓ | 107Cvl/s | ||
絕緣強(qiáng)度 | ASTM D-149 | 540↑ | v/mil | |||
體積電阻率 | ASTM D-257 | 1016↑ | Ω.cm | |||
熱性能 | 熱變形溫度 | 未退火 | 6.4mm 18.6kg/cm2 | ASTM D-648 | 96 | ℃ |
退火 | 6.4mm 18.6kg/cm2 | ASTM D-648 | 108 | ℃ | ||
維卡軟化點(diǎn) | ASTM D-1525 | 115 | ℃ |