規(guī)格級別 | 注塑級 |
|
產(chǎn)品簡述
規(guī)格級別 | 注塑級 |
詳細(xì)數(shù)據(jù)
訂購指南
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
物理性能 | 熔體流動速率 | 條件I | ASTM D-1238 | 14.0 | g/10min |
比重 | ASTM D-792 | 1.06 | 23/23℃ | ||
熔體流動速率 | 條件G | ASTM D-1238 | 2.8 | g/10min | |
機(jī)械性能 | 洛氏硬度 | ASTM D-785 | 83 | M | |
彎曲強(qiáng)度 | ASTM D-790 | 1000(14200) | kg/cm2(lb/in2) | ||
彎曲彈性率 | ASTM D-790 | 3.5(5.0) | 10kg/cm2(10lb/in2) | ||
伸長率 | ASTM D-638 | 3.0 | % | ||
IZOD沖擊強(qiáng)度 | 1/4〃 | ASTM D-256 | 1.7(0.31) | kg.cm/cm(ft.ld/in) | |
引張強(qiáng)度 | ASTM D-638 | 710(10060) | kg/cm2(lb/in2) | ||
IZOD沖擊強(qiáng)度 | 1/8〃 | ASTM D-256 | 1.8(0.33) | kg.cm/cm(ft.ld/in) | |
熱性能 | 熱變形溫度 | ASTM D-648 | 100(212) | ℃ | |
維卡軟化點(diǎn) | ASTM D-1525 | 104(219) | ℃(℉) | ||
熱變形溫度 | ASTM D-648 | 90(194) | ℉ | ||
燃燒性 | 1/16"HB |