斷裂伸長率 | 350% | 拉伸強度 | 53.77MPa | 密度 | 0.95g/cm3 |
熔體流動速率 | 11g/10min | 規(guī)格級別 | 擠出 | 缺口沖擊強度 | 150 |
加工級別 | 擠出級 |
|
產(chǎn)品簡述
斷裂伸長率 | 350% | 拉伸強度 | 53.77MPa | 密度 | 0.95g/cm3 |
熔體流動速率 | 11g/10min | 規(guī)格級別 | 擠出 | 缺口沖擊強度 | 150 |
加工級別 | 擠出級 |
詳細數(shù)據(jù)
訂購指南
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 密度 | ASTM D-792 | 0.950 | g/cm3 | ||
熔體流動速率 | 190℃/21.6kg | ASTM D-1238 | 11 | g/10min | ||
熔點 | DSC | 132 | ℃ | |||
機械性能 | 彎曲模量 | 1%正切 | ASTM D-790 | 813.5 | MPa | |
屈服拉伸強度 | MD | ASTM D-882 | 27.5 | MPa | ||
TD | ASTM D-882 | 24.13 | MPa | |||
斷裂拉伸強度 | MD | ASTM D-882 | 55.15 | MPa | ||
TD | ASTM D-882 | 53.77 | MPa | |||
斷裂伸長率 | MD | ASTM D-882 | 270 | % | ||
TD | ASTM D-882 | 350 | % | |||
缺口沖擊強度 | ASTM D-1709 | 150 | g | |||
埃爾曼多夫撕裂強度 | MD | ASTM D-1922 | 70 | g | ||
TD | ASTM D-1922 | 150 | g | |||
熱性能 | 維卡軟化點 | ASTM D-1525 | 124 | ℃ |