斷裂伸長率 | 720% | 拉伸強度 | 20.8MPa | 密度 | 0.923g/cm3 |
熔體流動速率 | 1.9g/10min | 用途級別 | 薄膜級 | 規(guī)格級別 | 薄膜 |
缺口沖擊強度 | 100 |
|
產(chǎn)品簡述
斷裂伸長率 | 720% | 拉伸強度 | 20.8MPa | 密度 | 0.923g/cm3 |
熔體流動速率 | 1.9g/10min | 用途級別 | 薄膜級 | 規(guī)格級別 | 薄膜 |
缺口沖擊強度 | 100 |
詳細數(shù)據(jù)
訂購指南
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 密度 | ASTM D-792 | 0.923 | g/cm3 | ||
熔體流動速率 | 190℃/2.16kg | ASTM D-1238 | 1.9 | g/10min | ||
薄膜厚度 | 50.8 | μ | ||||
機械性能 | 屈服拉伸強度 | MD | ASTM D-882 | 12.0 | MPa | |
TD | ASTM D-882 | 12.3 | MPa | |||
斷裂拉伸強度 | MD | ASTM D-882 | 24.8 | MPa | ||
TD | ASTM D-882 | 20.8 | MPa | |||
斷裂伸長率 | MD | ASTM D-882 | 520 | % | ||
TD | ASTM D-882 | 720 | % | |||
落鏢沖擊強度 | ASTM D-1709 | 100 | g | |||
埃爾曼多夫撕裂強度 | MD | ASTM D-1922 | 560 | g | ||
TD | ASTM D-1922 | 470 | g | |||
熱性能 | 維卡軟化點 | ASTM D-1525 | 92.2 | ℃ | ||
熔點 | DSC | 111 | ℃ | |||
其它性能 | 薄膜強硬 | MD | ASTM D-882 | 184 | J/cm3 | |
TD | ASTM D-882 | 190 | J/cm3 | |||
光學性能 | 光澤度 | 45° | ASTM D-2457 | 70 | ||
霧度 | ASTM D-1003 | 7.5 | % |