斷裂伸長率 | 860% | 密度 | 0.9g/cm3 | 熔體流動(dòng)速率 | 0.8g/10min |
維卡軟化點(diǎn) | 74℃ |
|
產(chǎn)品簡述
斷裂伸長率 | 860% | 密度 | 0.9g/cm3 | 熔體流動(dòng)速率 | 0.8g/10min |
維卡軟化點(diǎn) | 74℃ |
詳細(xì)數(shù)據(jù)
訂購指南
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 密度 | 23℃ | ASTM D-1505 | 0.900 | g/cm3 | |
熔體流動(dòng)速率 | ASTM D-1238 | 0.80 | g/10min | |||
機(jī)械性能 | 跌落沖擊強(qiáng)度 | ASTM D-1709 | >1,000 | g | ||
斷裂點(diǎn)伸張率 | 寬 | MD | ASTM D-882 | 750 | % | |
長 | TD | ASTM D-882 | 860 | % | ||
抗撕裂強(qiáng)度 | 寬 | MD | ASTM D-1922 | 340 | g | |
長 | TD | ASTM D-1922 | 500 | g | ||
破裂點(diǎn)張力 | 寬 | MD | ASTM D-882 | 315 | kg/cm2 | |
長 | TD | ASTM D-882 | 275 | kg/cm2 | ||
熱性能 | 軟化點(diǎn) | ASTM D-1525 | 74 | ℃ |