斷裂伸長率 | 750% | 拉伸強(qiáng)度 | 27MPa | 密度 | 0.919g/cm3 |
熔體流動速率 | 2.8g/10min | 維卡軟化點(diǎn) | 100℃ | 用途級別 | 薄膜級 |
規(guī)格級別 | 薄膜 |
|
產(chǎn)品簡述
斷裂伸長率 | 750% | 拉伸強(qiáng)度 | 27MPa | 密度 | 0.919g/cm3 |
熔體流動速率 | 2.8g/10min | 維卡軟化點(diǎn) | 100℃ | 用途級別 | 薄膜級 |
規(guī)格級別 | 薄膜 |
詳細(xì)數(shù)據(jù)
訂購指南
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 密度 | ASTM D-1505 | 0.919 | g/cm3 | ||
熔體流動速率 | ASTM D-1238 | 2.8 | g/10min | |||
物理性能 | 薄膜厚度 | ASTM D-746 | 25 | µm | ||
機(jī)械性能 | 斷裂伸長率 | MD | ASTM D-882 | 650 | % | |
TD | ASTM D-882 | 750 | % | |||
撕裂彈性率 | MD | ASTM D-882 | 2800 | Kg/cm2 | ||
TD | ASTM D-882 | 2800 | Kg/cm2 | |||
撕裂強(qiáng)度 | MD | ASTM D-1004 | 115 | Kg/cm | ||
TD | ASTM D-1004 | 105 | Kg/cm | |||
尖頭沖擊強(qiáng)度 | ASTM D-3420 | 3.5 | g/μm | |||
拉伸屈服強(qiáng)度 | MD | ASTM D-882 | 120 | Kg/cm2 | ||
TD | ASTM D-882 | 110 | Kg/cm2 | |||
拉伸斷裂強(qiáng)度 | MD | ASTM D-882 | 300 | Kg/cm2 | ||
TD | ASTM D-882 | 280 | Kg/cm2 | |||
熱性能 | 低溫脆化溫度 | ASTM D-746 | <-70 | ℃ | ||
維卡軟化點(diǎn) | ASTM D-1525 | 100 | ℃ |