斷裂伸長率 | 800% | 拉伸強(qiáng)度 | 40MPa | 密度 | 0.932g/cm3 |
熔體流動(dòng)速率 | 2.7g/10min | 維卡軟化點(diǎn) | 110℃ | 用途級別 | 薄膜級 |
規(guī)格級別 | 薄膜 |
|
產(chǎn)品簡述
斷裂伸長率 | 800% | 拉伸強(qiáng)度 | 40MPa | 密度 | 0.932g/cm3 |
熔體流動(dòng)速率 | 2.7g/10min | 維卡軟化點(diǎn) | 110℃ | 用途級別 | 薄膜級 |
規(guī)格級別 | 薄膜 |
詳細(xì)數(shù)據(jù)
訂購指南
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 密度 | ASTM D-1505 | 0.932 | g/cm3 | ||
熔體流動(dòng)速率 | ASTM D-1238 | 2.7 | g/10min | |||
物理性能 | 薄膜厚度 | 25 | µm | |||
機(jī)械性能 | 撕裂強(qiáng)度 | MD | ASTM D-1004 | 130 | kg/cm | |
TD | ASTM D-1004 | 120 | kg/cm | |||
斷裂伸長率 | MD | ASTM D-638 | 650 | % | ||
TD | ASTM D-638 | 800 | % | |||
拉伸屈服強(qiáng)度 | MD | ASTM D-638 | 180 | Kg/cm2 | ||
TD | ASTM D-638 | 170 | Kg/cm2 | |||
拉伸斷裂強(qiáng)度 | MD | ASTM D-638 | 440 | Kg/cm2 | ||
TD | ASTM D-638 | 410 | Kg/cm2 | |||
尖頭沖擊強(qiáng)度 | ASTM D-1709 | 4.2 | g/μm | |||
抗張模數(shù) | MD | ASTM D-882 | 3000 | Kg/cm2 | ||
TD | ASTM D-882 | 4000 | Kg/cm2 | |||
熱性能 | 維卡軟化點(diǎn) | ASTM D-1525 | 110 | ℃ | ||
低溫脆化溫度 | ASTM D-746 | <-80 | ℃ |