斷裂伸長率 | 830% | 拉伸強(qiáng)度 | 33MPa | 密度 | 0.918g/cm3 |
熔體流動(dòng)速率 | 2g/10min | 用途級別 | 薄膜級 | 規(guī)格級別 | 薄膜 |
|
產(chǎn)品簡述
斷裂伸長率 | 830% | 拉伸強(qiáng)度 | 33MPa | 密度 | 0.918g/cm3 |
熔體流動(dòng)速率 | 2g/10min | 用途級別 | 薄膜級 | 規(guī)格級別 | 薄膜 |
詳細(xì)數(shù)據(jù)
訂購指南
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 熔體流動(dòng)速率 | ASTM D-1238 | 2.0 | g/10min | ||
密度 | ExxonMobil Method | 0.918 | g/cm3 | |||
機(jī)械性能 | 極限伸長率 | MD | ASTM D-882 | 700 | % | |
TD | ASTM D-882 | 830 | % | |||
Elmendorf斷裂強(qiáng)度 | MD | ASTM D-1922 | 150 | g | ||
TD | ASTM D-1922 | 340 | g | |||
斷裂拉伸強(qiáng)度 | MD | ASTM D-882 | 5800 | psi(MPa) | ||
TD | ASTM D-882 | 4800 | psi(MPa) | |||
熱性能 | 熔點(diǎn) | ExxonMobil Method | 249(121) | ℉(℃) | ||
其它性能 | 擊穿 | ExxonMobil Method | 20 | in.lb | ||
計(jì)量 | ASTM D-374 | 1.2 | mil | |||
1%割線模量 | MD | ASTM D-882 | 28 | psi(MPa) | ||
TD | ASTM D-882 | 33 | psi(MPa) | |||
混濁度 | ASTM D-1003 | 18 | % | |||
屈服拉伸強(qiáng)度 | MD | ASTM D-882 | 1400 | psi(MPa) | ||
TD | ASTM D-882 | 1400 | psi(MPa) | |||
光澤度 | ASTM D-2457 | 40 |