加工級別 | 擠出級 |
|
產(chǎn)品簡述
加工級別 | 擠出級 |
詳細數(shù)據(jù)
訂購指南
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
基本性能 | 吸水率 | ASTM D-570 | 1.8 | % | |
吸水率 | ASTM D-570 | 10.7 | % | ||
成型收縮率 | UBEmethod | 1.3 | % | ||
成型收縮率 | UBEmethod | 1.4 | % | ||
物理性能 | 比重 | ASTM D-792 | 1.14 | ||
機械性能 | 硬度(洛氏、布氏) | 23° | ASTM D-785 | 120 | |
線性熱膨脹系數(shù) | ASTM D-696 | 8 | X的10-5cm/cm/°C | ||
彎曲彈性率 | -30° | ASTM D-790 | 35000 | kgf/cm2 | |
抗沖擊強度 | 23° | ASTM D-256 | 50 | kgf.cm/cm | |
彎曲強度 | 23° | ASTM D-790 | 1100 | kgf/cm2 | |
彎曲彈性率 | 23° | ASTM D-790 | 7000 | kgf/cm2 | |
1%變形下的壓縮強度 | 23° | ASTM D-695 | 200 | kgf/cm2 | |
彎曲強度 | 80° | ASTM D-790 | 400 | kgf/cm2 | |
彎曲強度 | -30° | ASTM D-790 | 1400 | kgf/cm2 | |
彎曲強度 | 80° | ASTM D-790 | 250 | kgf/cm2 | |
彎曲強度 | -30° | ASTM D-790 | 1300 | kgf/cm2 | |
擠剪強度 | 23° | ASTM D-732 | 650 | kgf/cm2 | |
抗沖擊強度 | 23° | ASTM D-256 | 7.5 | kgf.cm/cm | |
彎曲彈性率 | 80° | ASTM D-790 | 7000 | kgf/cm2 | |
彎曲彈性率 | 23° | ASTM D-790 | 25000 | kgf/cm2 | |
抗沖擊強度 | -30° | ASTM D-256 | 5.0 | kgf.cm/cm | |
硬度(洛氏、布氏) | 23° | ASTM D-785 | 85 | ||
彎曲強度 | 23° | ASTM D-790 | 400 | kgf/cm2 | |
屈服下的伸張強度 | 23° | ASTM D-638 | 400 | kgf/cm2 | |
硬度(洛氏、布氏) | 23° | ASTM D-785 | 55 | ||
斷裂下的延伸率 | 23° | ASTM D-638 | >200 | % | |
1%變形下的壓縮強度 | 23° | ASTM D-695 | 100 | kgf/cm2 | |
擠剪強度 | 23° | ASTM D-732 | 600 | kgf/cm2 | |
TABER磨耗率 | ASTM D-1044 | 7 | mg | ||
屈服下的伸張強度 | 23° | ASTM D-638 | 750 | kgf/cm2 | |
屈服下的伸張強度 | 80° | ASTM D-638 | 320 | kgf/cm2 | |
彎曲彈性率 | -30° | ASTM D-790 | 33000 | kgf/cm2 | |
斷裂下的伸張強度 | 23° | ASTM D-638 | >720 | kgf/cm2 | |
彎曲彈性率 | 80° | ASTM D-790 | 4000 | kgf/cm2 | |
屈服下的伸張強度 | -30° | ASTM D-638 | 870 | kgf/cm2 | |
屈服下的伸張強度 | -30° | ASTM D-638 | 1100 | kgf/cm2 | |
屈服下的延伸率 | 23° | ASTM D-638 | 8 | % | |
屈服下的伸張強度 | 80° | ASTM D-638 | 180 | kgf/cm2 | |
熱性能 | 熔點 | DSC | 215-225 | °C | |
熱變形溫度 | 18.6kgf/cm2 | ASTM D-648 | 65 | °C | |
熱變形溫度 | 4.6kgf/cm2 | ASTM D-648 | 170 | °C |