性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | ||||
基本性能 | 吸水率 | 23℃ | ASTM D-570 |
|
% | |||
物理性能 | 比重 | ASTM D-792 |
|
|||||
泰伯磨耗量 | (1000g,CS-17)23℃ | ASTM D-1044 |
|
mg/1000次 | ||||
機(jī)械性能 | 壓縮強(qiáng)度 | 23℃ | ASTM D-695 |
|
Kg/cm2 | |||
IZOD沖擊強(qiáng)度 | -40℃ |
|
kg·cm/cm2 | |||||
洛氏硬度 | 23℃ | ASTM D-785 |
|
R-標(biāo)度 | ||||
斷裂伸長(zhǎng)率 | -40℃ | ASTM D-638 |
|
% | ||||
斷裂伸長(zhǎng)率 | 80℃ | ASTM D-638 |
|
% | ||||
撓曲模量 | -40℃ | ASTM D-790 |
|
Kg/cm2 | ||||
抗剪強(qiáng)度 | 23℃ | ASTM D-732 |
|
Kg/cm2 | ||||
抗拉屈服強(qiáng)度 | 80℃ | ASTM D-638 |
|
Kg/cm2 | ||||
抗拉屈服強(qiáng)度 | -40℃ | ASTM D-638 |
|
Kg/cm2 | ||||
洛氏硬度 | 23℃ | ASTM D-785 |
|
M-標(biāo)度 | ||||
撓曲強(qiáng)度 | 80℃ | ASTM D-790 |
|
Kg/cm2 | ||||
撓曲強(qiáng)度 | -40℃ | ASTM D-790 |
|
Kg/cm2 | ||||
撓曲模量 | 80℃ | ASTM D-790 |
|
Kg/cm2 | ||||
IZOD沖擊強(qiáng)度 | -40℃,V缺口1/2 | ASTM D-256 |
|
kg·cm/cm | ||||
壓縮強(qiáng)度 | -40℃ | ASTM D-695 |
|
Kg/cm2 | ||||
IZOD沖擊強(qiáng)度 | 23℃,無缺口1/8 |
|
kg·cm/cm2 | |||||
斷裂伸長(zhǎng)率 | 23℃ | ASTM D-638 |
|
% | ||||
撓曲強(qiáng)度 | 23℃ | ASTM D-790 |
|
Kg/cm2 | ||||
抗剪強(qiáng)度 | 80℃ | ASTM D-732 |
|
Kg/cm2 | ||||
IZOD沖擊強(qiáng)度 | 23℃,V-缺口1/2 | ASTM D-256 |
|
kg·cm/cm | ||||
壓縮強(qiáng)度 | 80℃ | ASTM D-695 |
|
Kg/cm2 | ||||
抗拉屈服強(qiáng)度 | 23℃ | ASTM D-638 |
|
Kg/cm2 | ||||
電氣性能 | 抗電弧性 | 1/8" | ASTM D-495 |
|
s | |||
損耗因數(shù) | 103Hz | ASTM D-150 |
|
|||||
介電常數(shù) | 106Hz | ASTM D-150 |
|
|||||
介電強(qiáng)度 | 1/8" | ASTM D-149 |
|
KV/mm | ||||
介電常數(shù) | 103Hz | ASTM D-150 |
|
|||||
介電常數(shù) | 50Hz | ASTM D-150 |
|
|||||
體積電阻率 | ASTM D-257 |
|
Ω.cm | |||||
損耗因數(shù) | 50Hz | ASTM D-150 |
|
|||||
損耗因數(shù) | ASTM D-150 |
|
||||||
熱性能 | 比熱 |
|
Cal/g·℃ | |||||
UL-94抗燃級(jí) | 1/16" | UL 94 |
|
|||||
導(dǎo)熱系數(shù) |
|
Kcal/m·hr·℃ | ||||||
熱撓曲溫度 | 4.6kg/cm2 | ASTM D-648 |
|
℃ | ||||
熱撓曲溫度 | 18.6kg/cm2 | ASTM D-648 |
|
℃ | ||||
熔點(diǎn) | 差示掃描測(cè)熱計(jì)DSC |
|
℃ | |||||
線性熱膨脹系數(shù) | ASTM D-696 |
|
×10-5cm/cm/℃ | |||||
其它性能 | 強(qiáng)化含量 |
|
WT% |