密度 | 1.53g/cm3 | 彎曲強(qiáng)度 | 156.8MPa | 吸水率 | 0.07% |
彎曲模量 | 6076MPa | 缺口沖擊強(qiáng)度 | 5 |
|
產(chǎn)品簡(jiǎn)述
密度 | 1.53g/cm3 | 彎曲強(qiáng)度 | 156.8MPa | 吸水率 | 0.07% |
彎曲模量 | 6076MPa | 缺口沖擊強(qiáng)度 | 5 |
詳細(xì)數(shù)據(jù)
訂購(gòu)指南
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
物理性能 | ??s系數(shù) | 4-14 | cm/cm×0.0001 | |||
比重 | ASTM D-792 | 1.53 | ||||
吸水率 | ASTM D-570 | 0.07 | % | |||
機(jī)械性能 | 彎曲強(qiáng)度 | ASTM D-790 | 1600 | kg/cm2 | ||
彎曲模數(shù) | ASTM D-790 | 62000 | kg/cm2 | |||
伸張力 | ASTM D-638 | 4.0 | % | |||
洛氏硬度 | ASTM D-785 | 90 | M(R) | |||
磨擦系數(shù) | ASTM D-1984 | 0.13 | ||||
拉力 | ASTM D-638 | 1100 | kg/cm2 | |||
沖擊強(qiáng)度 | 缺口 | ASTM D-256 | 5.0 | kg.cm/cm | ||
無(wú)缺口 | ASTM D-256 | 30 | kg.cm/cm | |||
電氣性能 | 抗弧性 | ASTM D-495 | 50 | Sec | ||
誘電正接 | 106HZ | ASTM D-150 | 0.02 | |||
介電定數(shù) | 106HZ | ASTM D-150 | 3.4 | |||
抗體積性 | ASTM D-257 | >1016 | Ω.cm | |||
介電定數(shù) | 100HZ | ASTM D-150 | 3.6 | |||
誘電正接 | 100HZ | ASTM D-150 | 0.002 | |||
介電強(qiáng)度 | ASTM D-149 | 27 | KV/mm | |||
熱性能 | 防燃性 | V-0(1/32") | ||||
熱折射溫度 | 18.6kg/cm2 | ASTM D-648 | 210 | ℃ | ||
熱折射溫度 | 18.6kg/cm2 | ASTM D-648 | 200 | ℃ | ||
線熱伸張系數(shù) | ASTM D-696 | 5×0.000005 | mm/mm/℃ |