性能項(xiàng)目 | 測試條件 | 測試方法 | 數(shù)值/描述 | 單位 | |
機(jī)械性能 | 拉伸強(qiáng)度(引張強(qiáng)度) | ASTM D638/ISO 527 | 62.7 | kg/cm²(MPa)[Lb/in2] | |
斷裂伸長率 | ASTM D638/ISO 527 | 40 | % | ||
拉伸模量 | ASTM D638/ISO 527 | -- | kg/cm²(MPa)[Lb/in2] | ||
拉伸屈服伸長率(延伸率) | ASTM D638/ISO 527 | -- | % | ||
拉伸斷裂伸長率(延伸率) | ASTM D638/ISO 527 | -- | % | ||
彎曲模量(彎曲彈性率) | ASTM D790/ISO 178 | 2650 | kg/cm²(MPa)[Lb/in2] | ||
彎曲強(qiáng)度 | ASTM D790/ISO 178 | 102 | kg/cm²(MPa)[Lb/in2] | ||
洛氏硬度 | ASTM D785 | R-123 | |||
IZOD 缺口沖擊強(qiáng)度 | 1/4" 23℃ | ASTM D256/ISO 179 | 534 | kg·cm/cm(J/M)ft·lb/in | |
1/4" -30℃ | ASTM D256/ISO 179 | 160 | kg·cm/cm(J/M)ft·lb/in | ||
1/8" 23℃ | ASTM D256/ISO 179 | -- | kg·cm/cm(J/M)ft·lb/in | ||
1/8" -30℃ | ASTM D256/ISO 179 | -- | kg·cm/cm(J/M)ft·lb/in | ||
Charpy沖擊強(qiáng)度 | 23℃ (缺口) | ASTM D256/ISO 179 | -- | kg·cm/cm(J/M)ft·lb/in | |
-30℃(缺口) | ASTM D256/ISO 179 | -- | kg·cm/cm(J/M)ft·lb/in | ||
23℃(無缺口) | ASTM D256/ISO 179 | -- | kg·cm/cm(J/M)ft·lb/in | ||
-30℃(無缺口) | ASTM D256/ISO 179 | -- | kg·cm/cm(J/M)ft·lb/in | ||
物性性能 | 比重(密度) | ASTM D792/ISO 1183 | 1.18 | ||
成型收縮率 | ASTM D955 | 0.4-0.6 | % | ||
熔融指數(shù)(流動系數(shù)) | 200℃/5kg | ASTM D1238/ISO 1133 | 260℃/2.16Kg,10 | g/10min | |
220℃/10kg | ASTM D1238/ISO 1133 | -- | g/10min | ||
吸水率 23℃/24H | ASTM D570/ISO 62 | 0.1-0.4 | % | ||
熱性能 | 熱變形溫度 | 退火 | ASTM D648/ISO 75 | -- | ℃(℉) |
未退火 | ASTM D648/ISO 75 | 0.45MPa/6.40mm,104℃;1.80MPa/6.40mm,95.0℃ | ℃(℉) | ||
維卡軟化點(diǎn) | ASTM D1525/ISO R306 | 113 | ℃(℉) | ||
熔點(diǎn) | - | -- | ℃(℉) | ||
燃燒性(率) | UL94 | 1.50mm,V-0;2.49mm,5VB | |||
線性膨脹系數(shù) | ASTM D696/ISO 11359 | 0.072*10^-6 | mm/mm.℃ | ||
電氣性能 | 介電常數(shù) | 100HZ | ASTM D150/IEC 60250 | 3.00 | |
1MHZ | ASTM D150/IEC 60250 | -- | |||
體積電阻率 | ASTM D257/IEC 60093 | >1.0E+17 ohms.cm | Ω.cm | ||
表面電阻率 | ASTM D257/IEC 60093 | >1.0E+16 ohms | Ω | ||
耐電弧性 | ASTM D495/IEC 60112 | PLC6 | |||
加工條件 | 干燥條件 | ||||
加工溫度 | 射嘴 | ℃ | |||
料筒前段 | ℃ | ||||
料筒中段 | ℃ | ||||
料筒后段 | ℃ | ||||