詳細(xì)數(shù)據(jù)
訂購指南
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | |
物理性能 | 熔融指數(shù) | 260℃,5kg | ASTM D-1238 | 30 | g/10min |
密度 | ASTM D-1505 | 1.08 | g/cm3 | ||
熔點(diǎn) | MCI方法 | 240 | ℃ | ||
機(jī)械性能 | 抗張強(qiáng)度 | ASTM D-638 | 170 | kg/cm2 | |
凹口Charpy耐沖擊強(qiáng)度 | ASTM D-256 | --- | kgcm/cm2 | ||
斷裂伸長(zhǎng)率 | ASTM D-638 | 25 | % | ||
曲折模數(shù) | ASTM D-790 | 19,000 | kg/cm2 | ||
抗張屈服強(qiáng)度 | ASTM D-638 | 240 | kg/cm2 | ||
Rockwell硬度 | ASTM D-785 | R90 | |||
無凹口lzod耐沖擊強(qiáng)度 | ASTM D-256 | -- | kgcm/cm2 | ||
曲折強(qiáng)度 | ASTM D-790 | 390 | kg/cm2 | ||
Olsen剛性 | ASTM D-747 | --- | kg/cm2 | ||
電氣性能 | 介電常數(shù) | 100~1MHz | ASTM D-150 | --- | |
吸水率 | 24hr | ASTM D-570 | 0.11 | % | |
介電強(qiáng)度 | ASTM D-149 | --- | KV/mm | ||
體積電阻系數(shù) | ASTM D-257 | --- | Ωcm | ||
介電消散因子 | 23℃,1MHz | ASTM D-150 | 0.0014 | ||
熱性能 | 比熱 | ASTM C-351 | --- | cal/g℃ | |
燃燒速率 | ASTM D-635 | --- | cm/min | ||
Vicat軟化點(diǎn) | ASTM D-1525 | 175 | ℃ | ||
熱變形溫度 | 4.6kg/cm2 | ASTM D-648 | 110 | ℃ | |
熱傳導(dǎo)系數(shù) | ASTM BS-847A | --- | calcm/seccm2℃ | ||
模收縮率(機(jī)械/垂直方向) | MCI方法 | 1.7/1.4 | % | ||
線膨脹系數(shù) | ASTM D-696 | --- | 1/℃ | ||
其它性能 | 折射率 | ASTM D-542 | --- | nd | |
模糊度 | ASTM D-1746 | --- | % | ||
透光率 | ASTM D-1746 | --- | % |